Zduńska fireclay mortar ZSZ2/III
- Factory prepared dry mixture of refractory wedges and sorted aggregates szamotowego.
Designed to combine - prostek, tile kilns in the refractory tile, fireplaces, heating stoves of individual and small dokonywnaia repair.
- After burning resistant to temperatures up to 1300 o C.
- are delivered to the recipient in the dry state. On site to earn them with water. For mortar ZSZ2/III used to the temperature of 1000 o C it is advisable to introduce additives spiekające ie water glass sodium or Portland cement, which act as a flux to facilitate sintering. < / li>
- Store in dry and undamaged packaging, indefinitely.
Specifications:
Chemical analysis
AI 2 O 3
Fe 2 O 3 |
% |
28.00
3.00 |
texture |
mm |
0.00 - 2.0 |
Content nadziarna |
% |
<5 |
Refractoriness |
o C |
1670 |
ZSZ2/III Packaging: 5 kg, 10 kg; 25 kg
|